FCW-Sw-35Cr6Mo2
|
|
GOST 26101-84 EN 14700/ DIN 8555/ (suspended)
|
Welding process: S – under the flux |
Wire diameter, mm | Recommended shielding gases and fluxes |
S | 1,6–3,6 |
The Formation of the weld bead | good |
Separation of Slag | good |
Deposition Rate, kg/h | 5-19 |
Addiction Weld metal Cracking | moderate |
Consumption per 1 kg of wire Weld metal, kg | 1.05-1.05 |
Weld metal Hardness (HRC for 3rd-4th layer, unless otherwise stated) | after surfacing 44-55 |
Wire diameter, mm |
Current, A |
Voltage, V |
Surfacing rate, m/h |
1,6 – 1,8 |
160 – 240 |
27 – 29 |
10 - 15 |
2,0 – 2,2 |
180 – 260 |
28 – 30 |
12 - 18 |
2,4 – 2,6 |
200 – 320 |
29 – 31 |
15 - 20 |
2,8 – 3,0 |
260 – 350 |
30 – 32 |
18 - 23 |
3,2 – 3,4 |
300 – 400 |
30 – 32 |
20 – 25 |
3,6 |
340 - 450 |
31 - 33 |
20 - 25 |
C | Cr | Mo | Ti | V | N | S | P |
0.4 | 7.0 | 2.5 | 0.08 | 0.6 | 0.03 | 0.03 | 0.03 |
Brand of the wire | Distance, % | virobnik | C | Mn | Si | Cr | Mo | Ti | W | V |
ROBOTOOL 58-G (21) | 1.48 | Welding Alloys | 0.35 | 1.2 | 0.5 | 7 | 2.2 | 0.3 | ||
ROBOTOOL 46-G (19) | 1.87 | Welding Alloys | 0.2 | 0.9 | 0.5 | 6 | 3.5 | 0.25 | ||
ROBOTOOL 47-G (20) | 1.87 | Welding Alloys | 0.15 | 0.9 | 0.5 | 6 | 3.5 | 0.25 | ||
HARDFACE WMOLC (26) | 2.35 | Welding Alloys | 0.3 | 0.9 | 0.6 | 6.5 | 2.2 | 2 | 0.6 | |
ROBODUR K 600-G (12) | 2.56 | Welding Alloys | 0.5 | 1.2 | 0.7 | 6 | 0.7 |
Wire diameter, mm | Cardboard barrel | Molded skeins of frameless type | Frame drum (B) | Coil (S), (BS) | |||
Hank in the corrugation box | Metallic barrel | ||||||
To 100 kg | To 150 kg | To 300 kg | To 30 kg | To 70 kg | To 25 kg | To 15 kg | |
1.6 | X | X | X | X | X | X | X |
2.0 | X | X | X | X | X | X | X |
2.4 | X | X | X | X | X | X | X |
2.8 | X | X | X | X | X | X | |
3.0 | X | X | X | X | X | X | |
3.2 | X | X | X | X | X | X | |
3.6 | X | X | X | X | X | X |