Wet-FCW-Sw-14MnSiTi
|
|
TUU 19369185.013-97 EN 14700/ DIN 8555/ (suspended)
|
Welding process: О – open arc |
Wire diameter, mm | Recommended shielding gases and fluxes |
О | 1,6–3,0 | - |
The Formation of the weld bead | good |
Separation of Slag | good |
Deposition Rate, kg/h | 5-10 |
Addiction Weld metal Cracking | moderate |
Consumption per 1 kg of wire Weld metal, kg | 1.15-1.25 |
Weld metal Hardness (HRC for 3rd-4th layer, unless otherwise stated) | after surfacing HB 230-HB 280 |
Wire diameter, mm |
Current, A |
Voltage, V |
Surfacing rate, m/h |
1,6 – 1,8 |
140 – 240 |
24 – 26 |
10 - 15 |
2,0 – 2,2 |
180 – 280 |
25 – 27 |
12 - 18 |
2,4 – 2,6 |
220 – 320 |
26 – 28 |
15 - 20 |
2,8 – 3,0 |
260 – 350 |
26 – 28 |
18 - 23 |
C | Mn | Si | Ti | S | P |
0.14 | 0.5 | 0.5 | 0.4 | 0.03 | 0.03 |
Brand of the wire | Distance, % | virobnik | C | Mn | Si | Mo |
ROBOFIL R 71+ (52) | 0.82 | Welding Alloys | 0.04 | 1.2 | 0.4 | |
ROBOFIL KX71T1+ (53) | 0.9 | Welding Alloys | 0.05 | 1.3 | 0.5 | |
ROBOFIL M Mo (70) | 0.96 | Welding Alloys | 0.06 | 1.2 | 0.4 | 0.5 |
ROBOFIL M 71 (55) | 0.99 | Welding Alloys | 0.07 | 1.4 | 0.5 | |
ROBOFIL B 71 (56) | 0.99 | Welding Alloys | 0.06 | 1.4 | 0.4 |
Wire diameter, mm | Cardboard barrel | Molded skeins of frameless type | Frame drum (B) | Coil (S), (BS) | |||
Hank in the corrugation box | Metallic barrel | ||||||
To 100 kg | To 150 kg | To 300 kg | To 30 kg | To 70 kg | To 25 kg | To 15 kg | |
1.6 | X | X | X | X | X | X | X |
2.0 | X | X | X | X | X | X | X |
2.4 | X | X | X | X | X | X | X |
2.8 | X | X | X | X | X | X | |
3.0 | X | X | X | X | X | X |